Glossary

Hydrogen porosity in aluminium welding

Hydrogen porosity in aluminium welding

Hydrogen porosity refers to gas pores that may form as an aluminium weld solidifies. Hydrogen is considerably more soluble in molten aluminium than in the solid metal. During solidification, excess hydrogen may form pores if it cannot escape in time. Potential sources include moisture, contamination on the base material or filler wire, and unsuitable shielding-gas or process conditions. Clean, dry surfaces, suitable filler materials and correctly adjusted welding parameters help reduce the risk. The cause should be assessed in the context of the specific welding process.

WeldGuard helps assess common welding defects

Berkenhoff GmbH (headquarters)

  • Kinzenbach plant
  • Berkenhoffstraße 14
  • 35452 Heuchelheim
  • Germany

Berkenhoff GmbH

  • Merkenbach plant
  • Rehmühle 1
  • 35745 Herborn
  • Germany

bedra Vietnam Alloy Material Co., Ltd

  • Lot CN-06, Hoa Phu Industrial Park,
    Xuan Cam Commune,
    Bac Ninh City,
    Vietnam
  • +84 2043900104
  • info-asia(at)bedra.com
Close

You are about to leave the bedra Europe website

Back Visit

Service