bercoweld® K8 is made of copper silver material. Especially suitable for buildup and join welding on copper; preheat to about 450° C for large workpieces.
| ISO 24373 | CuAg1 Cu1897 |
|---|---|
| Cu | balance |
| Ag | 0.80 - 1.00 |
| P | 0.025 - 0.050 |
| Mn | 0.05 - 0.12 |
| Others | max. 0.5 |
| Density (kg/dm³) | 8.9 |
|---|---|
| Melting range (°C) | 1070 - 1080 |
| Thermal conductivity (W / m x K) | 220 - 315 |
| Coefficient of linear mean expansion (10-6/K) | 17.7 |
| Electric conductivity (m / Ω x mm²) | 38 - 40 |
| Resistivity (Ω x mm² /m) | 0.025 - 0.0263 |
| Heat treatment | non treated |
|---|---|
| Tensile strength (MPa) | 200 |
| Elongation (%) | 30 |
| Brinell hardness (HB 2.5/62.5) | 60 |
| Notched bar impact test (Av (J)) | 75 |
| Make-up | Weight/Length | Dimension |
|---|---|---|
| Drum / bedrabox | 175 - 200 kg | 0.80 - 1.60 mm |
| SD300 / BS300 / K300 | 12 - 15 kg | 0.80 - 2.40 mm |
| H500 / H560 / H760 | 150 - 250 kg | 0.80 - 2.40 mm |
| Coils | 25 - 100 kg | 1.60 - 6.00 mm |
| Rodse | 250 - 3000 mm | 1.60 - 6.00 mm |
PDF Datasheet | EN PDF Datasheet | DE